November 3, 2022
|
No-Clean Residue Shorts
We have a PCBA with a QFN 44 using no-clean flux. We have many test failures during testing. Are the failures due to flux reside between terminations? The Assembly Brothers, Phil Zarrow and Jim Hall, answer this question and share their own experiences.
Board Talk
|
|
|
|
Solder Paste Life on the Stencil
Our solder paste has a specified life for exposure on the stencil at 10 hours. We run our stencil operation continuously for 40 hours, adding 250g of new paste ...
Ask the Experts
|
|
|
|
|
|
|
|
ESD and Humidification
In the handling of circuit board assemblies placing them into systems, is ambient air humidification necessary if other means of protection are enforced including ESD ...